Solvent based gravure inks for surface printing, non laminating.
2. Name                     : Q-Surf3. Features and Uses:-	MulT Surf A is a type of gravure ink system, was applied for treated PE, PP film (with surface tension more than 38 dyne/cm)
-     High gloss
-     Good adhesion on film
-     Good blocking resistance, abrasion resistance
-     Good ink transfer and printability
-     Leave less residual solvent
4. Main Compositions:-     Resin     : Polyamide
-     Pigment : Organic/ Inorganic pigment
-     Additive : Synthetic wax
-     Solvent  : Toluene / Isopropanol (IPA) 
5. Physical Properties:
 
  | 
     
    
  Colour 
   | 
  
     
    
  Code 
   | 
  
     
  Net weight (kg) 
   | 
  
     
    
  Viscosity 
  (sec) 
   | 
  
   Light fastness 
   | 
  
     
    
  Water 
  Resistance 
   | 
  
     
  Acid& Alkali
  Resistance 
   | 
 
 
  | 
     
  Full 
   | 
  
     
  Tint 
   | 
 
 
  | 
   White 
   | 
  
   W001 
   | 
  
   20 
   | 
  
   25÷ 55 
   | 
  
   AA 
   | 
  
   AA 
   | 
  
   A 
   | 
  
   A 
   | 
 
 
  | 
   Yellow 
   | 
  
   Y203 
   | 
  
   17 
   | 
  
   25÷ 60 
   | 
  
   B 
   | 
  
   C 
   | 
  
   A 
   | 
  
   A 
   | 
 
 
  | 
   Red 
   | 
  
   R106 
   | 
  
   17 
   | 
  
   30÷ 65 
   | 
  
   B 
   | 
  
   C 
   | 
  
   A 
   | 
  
   A 
   | 
 
 
  | 
   Orange 
   | 
  
   O307B 
   | 
  
   17 
   | 
  
   30÷ 65 
   | 
  
   B 
   | 
  
   C 
   | 
  
   A 
   | 
  
   A 
   | 
 
 
  | 
   Green 
   | 
  
   Gr401 
   | 
  
   17 
   | 
  
   25÷ 60 
   | 
  
   AA 
   | 
  
   A 
   | 
  
   A 
   | 
  
   A 
   | 
 
 
  | 
   Blue 
   | 
  
   B301 
   | 
  
   17 
   | 
  
   25÷ 55 
   | 
  
   AA 
   | 
  
   A 
   | 
  
   A 
   | 
  
   A 
   | 
 
 
  | 
   Violet 
   | 
  
   V703 
   | 
  
   17 
   | 
  
   25÷ 55 
   | 
  
   A 
   | 
  
   B 
   | 
  
   A 
   | 
  
   A 
   | 
 
 
  | 
   Black 
   | 
  
   BL501 
   | 
  
   17 
   | 
  
   25÷ 60 
   | 
  
   AA 
   | 
  
   A 
   | 
  
   A 
   | 
  
   A 
   | 
 
 
  | 
   Medium 
   | 
  
   Me 
   | 
  
   17 
   | 
  
   20÷ 40 
   | 
  
     
   | 
  
     
   | 
  
     
   | 
  
     
   | 
 
Remark:
- Fineness: < 10 microns
- Viscosity: measured by Zahn No.3 Jis
- Acid resistance:
Dipping into solutions of 3% hydrochloric acid and 7% acetic acid; slightly colouring of solution, but no change in shade of ink film after 30 mins.
- Alkali resistance:
Same result as acid test after 30 mins. Dipping into solution of 2% NaOH at room temperature.
- Water resistance:
Same result as acid test after 30 mins. Dipping into water at room temperature.
A          : No change
B          : Slightly colouring of solution but no change of shade of ink film
C          : Slightly fading of shade of ink film and a little colouring of the solution
D          : Fading pretty much
- Light fastness:
Tester: Sun Tester 575
Distance from light source to substance: 300 mm
     Full: high concentration (colour ink : white ink = 1: 0)
     Tint: low concentration (colour ink : white ink = 1:10)
The degree of resistance:
AA        : No fading after 60 hours
A          : Fading after 35 - 60 hours
B          : Fading after 15 - 35 hours
C          : Slightly fading after 15 hours
D          : Fading much within 15 hours
6.Thinner:
 
 
  | 
     
   | 
  
   Printing  speed  (m/min) 
   | 
  
     
  Toluene 
   | 
  
     
  IPA 
   | 
  
     
  EA 
   | 
  
     
  MEK 
   | 
  
     
  BA 
   | 
 
 
  | 
   Slow drying 
   | 
  
   <100 
   | 
  
   60 
   | 
  
   30 
   | 
  
     
   | 
  
   0.5 
   | 
  
   0.5 
   | 
 
 
  | 
   Quick drying 
   | 
  
   >100 
   | 
  
   60 
   | 
  
   30 
   | 
  
   10 
   | 
  
     
   | 
  
     
   | 
 
 
 
 
Note: EA : Ethyl Acetate, BA: Butyl Acetate, MEK : Methyl Ethyl Ketone, IPA: Isopropyl Alcohol
7. Attention for Users:
-     Stir well before using.
-	The fineness of previously used inks should be tested before using because a long-term storage can cause an ink agglomerate. Only mix 10 – 30 % previously used inks into fresh inks and sieve carefully by filter screen 100 µm or metal screen 120 mesh.
-	Using  the ink supply system  together filter screen equipment and circulating  pump to prevent inks from skinning, foreign matters as well as to stabilize colour strength.
-	For the printing with less ink consumption and small printing plate, moisture can be easily introduced due to long contact with air, leading to thickening and filling-in. To prevent these phenomena, slow drying solvent should be used in so far as possible, and humidity of working areas should be controlled at 55 – 65%.
-    Ensuring a good blocking resistance, it’s necessary to control adequate drying rate.
Medium usage:
For printing, medium is added into inks to decrease colour strength, depends on the cell- deepness of cylinders. Generally, 10 – 15% medium should be mixed into fresh inks. In special cases, the medium content used is a higher ratio. We recommend the medium ratio as follows:
    Medium rate ≤ 10 – 15% : using non – additives Medium.
    Medium rate  > 15%       : using Medium with additives.
8. Safety and storage information:
-		The  products  contain  flammable  liquids.  Thus,  it’s  necessary  to  keep  a  working  area ventilating or install a exhaust system of ventilation. Keep away from heat, spark/flame, and static electricity.
-     Storage and handling at 15 – 25oC.
-     Avoid contact with skin and eyes.
-     Shelf life: 6 months after date of manufacture (in condition 15 – 25oC).